このエントリーをはてなブックマークに追加
ID 68698
フルテキストURL
fulltext.pdf 2.21 MB
著者
Maruo, Yukinori Department of Prosthodontics, Okayama University ORCID Kaken ID publons researchmap
Kuwahara, Miho Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Yoshihara, Kumiko Health Research Institute, National Institute of Advanced Industrial Science and Technology
Irie, Masao Department of Biomaterials, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences Kaken ID publons researchmap
Nagaoka, Noriyuki Advanced Research Center for Oral and Craniofacial Sciences, Okayama University Dental School
Yoshizane, Mai Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Matsumoto, Takuya Department of Biomaterials, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences Kaken ID researchmap
Akiyama, Kentaro Department of Occlusal and Oral Functional Rehabilitation, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
抄録
This study investigated the effects of varying concentrations of two distinct silane agents, 8-methacryloxyoctyl trimethoxy silane (8-MOTS) and 3-methacryloxypropyl trimethoxy silane (γ-MPTS), on their initial bonding efficacy to feldspathic ceramic (FC), lithium disilicate glass-ceramic (LD) and polymer-infiltrated ceramic (PIC) specimens, in 10% increments for concentrations ranging from 10% to 40%. Shear bond strengths between the ceramic substrates and the luting material were assessed following 24 h incubation in distilled water. For FC, the median value of shear bond strength peaked at 20% of γ-MPTS (7.4 MPa), while 8-MOTS exhibited a concentration-dependent increase, reaching its highest value at 40% (13.1 MPa). For LD, γ-MPTS above 10% yielded similar strength median values (10.2 MPa), whereas 8-MOTS at 30% (15.8 MPa) and 40% (13.4 MPa) yielded higher strength values than at 10% (2.9 MPa) and 20% (4.1 MPa), with the highest median value exhibited at 30%. For PIC, both γ-MPTS and 8-MOTS demonstrated similarly low bond strength values which were not significantly different from the non-silane-treated specimens. When applied on silica-based FC and LD, silane revealed a concentration-dependent bonding effect, with 8-MOTS exhibiting superior bond strength to γ-MPTS. However, PIC, characterized by a high inorganic filler content, demonstrated limited bondability with both silanes.
キーワード
silane coupling
bond strength
ceramic
feldspathic
lithium
polymer-infiltrated ceramic
CAD/CAM
発行日
2025-04-27
出版物タイトル
Materials
18巻
9号
出版者
MDPI
開始ページ
1983
ISSN
1996-1944
資料タイプ
学術雑誌論文
言語
英語
OAI-PMH Set
岡山大学
著作権者
© 2025 by the authors.
論文のバージョン
publisher
PubMed ID
DOI
Web of Science KeyUT
関連URL
isVersionOf https://doi.org/10.3390/ma18091983
ライセンス
https://creativecommons.org/licenses/by/4.0/
Citation
Maruo, Y.; Kuwahara, M.; Yoshihara, K.; Irie, M.; Nagaoka, N.; Yoshizane, M.; Matsumoto, T.; Akiyama, K. Initial Bonding Performance to CAD/CAM Restorative Materials: The Impact of Stepwise Concentration Variation in 8-Methacryloxyoctyl Trimethoxy Silane and 3-Methacryloxypropyl Trimethoxy Silane on Feldspathic Ceramic, Lithium Disilicate Glass-Ceramic, and Polymer-Infiltrated Ceramic. Materials 2025, 18, 1983. https://doi.org/10.3390/ma18091983
助成機関名
Japan Society for the Promotion of Science
助成番号
JP24K13004