このエントリーをはてなブックマークに追加
ID 32846
JaLCDOI
フルテキストURL
fulltext.pdf 4.59 MB
著者
Mine, Yoshinari Department of Cardiovascular Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Mitsui, Hideya Department of Cardiovascular Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences
Oshima, Yu Department of Cardiovascular Surgery, Shin Tokyo Hospital
Noishiki, Yasuharu Division of Artificial Organs, Yokohama City University School of Medicine
Nakai, Mikizo Department of Cardiovascular Surgery, NHO Okayama Medical Center
Sano, Shunji Department of Cardiovascular Surgery, Okayama University Graduate School of Medicine, Dentistry and Pharmaceutical Sciences Kaken ID publons researchmap
抄録

Our meticulous investigation of ePTFE graft breakage when a wire placed at the edge of an ePTFE graft was pulled, revealed that, depending on the breakage pattern, a break starts much earlier than the peak suture retention strength, which is the current international indicator for anastomotic-site break strength. Furthermore, the breakage patterns differ based on the thickness of the wire and the fiber direction of the ePTFE graft. Based on these findings, we advocate measuring the peak suture retention strength using 0.10-mm sutures and a standardized wire thickness in order to assess the anastomotic retention strength of ePTFE grafts.

キーワード
ePTFE
suture retention strength
anastomotic strength
Amo Type
Original Article
出版物タイトル
Acta Medica Okayama
発行日
2010-04
64巻
2号
出版者
Okayama University Medical School
開始ページ
121
終了ページ
128
ISSN
0386-300X
NCID
AA00508441
資料タイプ
学術雑誌論文
言語
英語
論文のバージョン
publisher
査読
有り
PubMed ID
Web of Science KeyUT